QY533 matting agent (Indoor semi-chemical)
number:QY533
material quality:powder
colour:white
Category: powder coating additive
QY533 Indoor Semi-chemical Matting Agent
一.Description
QY533 is an indoor semi-chemical matting agent, with gloss below 5%, stable storage, selective for resin, and good applicability to 50/50 polyester.
二.Technical indicators:
Apprearance : white to light yellow powder
Bulk density [g/l]: 390-490
Solid content[%] : ≥99%
三. Product Features
QY533 is suitable for 50/50 polyester and has a certain effect on some 60/40 polyester. One part of matting agent consumes 2 parts of epoxy and is directly added to the extrusion.
- The addition amount is 2-5%, and the gloss is 2.8-9.5%.
- The surface is smooth and delicate, not yellowing.
- The baking temperature is 200℃ x 15 minutes
四. Dosage and Usage
It is 2-5% of the total weight of the formula, not more than 5%, mixed with all other components, extruded through the extruder, please control the extrusion temperature to be consistent, and the gloss decreases with the increase of the addition amoun.
五.Test reference formula:
QY533 matting agent test
Products | Test 1 | Test 2 | Test 3 | Test 4 |
Polyester (Guanghua 1156) | 25.5 | 24.5 | 23.5 | 22.5 |
Resin(Tianma) | 29.5 | 30.5 | 31.5 | 32.5 |
Brightener, leveling agent, benzoin | 2.5 | 2.5 | 2.5 | 2.5 |
Extinction barium | 40 | 39 | 38 | 37 |
QY533 Matting agent | 2 | 3 | 4 | 5 |
Carbon Black | 0.5 | 0.5 | 0.5 | 0.5 |
Total | 100 | 100 | 100 | 100 |
Screw speed (small prototype) | 38HZ | 38HZ | 38HZ | 38HZ |
Extrusion temperature Zone 1/Zone 2 | 100/110 | 100/110 | 100/110 | 100/110 |
Gloss | 11 | 4.5 | 3 | 2 |
Surface | smooth | exquisite | exquisite | exquisite |
Illustrate:
- It is not recommended to add accelerators to the formula to improve mechanical properties. It may cause an increase in gloss and deterioration in leveling. It is recommended to test it in a small test.
2.Polyesters from different manufacturers have different gloss, leveling, and gel time (Storage). It is recommended to test several polyesters.
3.The addition of accelerators may cause an increase in gloss and deterioration in leveling. It is recommended to test it in a small test.
- The baking temperature has a certain effect on the gloss stability. If the baking temperature is too low, the gloss may be high. It is recommended to ensure stable baking conditions.
六. Packaging and storage
Kraft paper bag (polyethylene lining), 25Kg/bag. Store in a cool and dry place, away from fire and heat sources.
the gloss may be high. It is recommended to ensure stable baking conditions.