Featured
QY532 matting agent(Indoor physical )
number:QY532
material quality:powder
colour:white
Category: powder coating additive
QY532 Indoor physical matting agent
一. Description:
QY532 Indoor physical matting agent, can achieve 2.5% matte, no need to change the formula, no yellowing, can reduce powder cost
二.Technical indicators:
Apprearance : white to light yellow powder
Bulk density [g/l]: 320-440
Solid content[%] : ≥99%
三. Product features
QY532 is suitable for 50/50 and 60/40. It is directly added to the internal extrusion. It is an additive physical matting agent and does not affect the original epoxy polyester ratio of the formula.
- The addition amount is 2-5%, and the gloss is 2.8-9.5%.
- The surface is smooth and delicate, without yellowing.
- The baking temperature is 190℃x15 minutes.
- The selectivity for polyester is relatively small. Most 50/50 polyesters and about half of 60/40 polyesters can obtain good matting effects.
四.Dosage and Usage
2-5% of the total weight of the formula, mixed with all other components, extruded through an Extruder, please control the extrusion temperature to be consistent, the gloss decreases with the increase of the added amount.
五.Test reference formula:
QY532 matting agent test
product | Test 1 | Test 2 | Test 3 | Test 4 |
Polyester (Guanghua 1156) | 27.5 | 27.5 | 27.5 | 27.5 |
Resin(Tianma) | 27.5 | 27.5 | 27.5 | 27.5 |
Brightener, leveling agent, Benzoin | 2.5 | 2.5 | 2.5 | 2.5 |
Extinction barium | 40 | 39 | 38 | 37 |
HC532 Matting agent | 2 | 3 | 4 | 5 |
Carbon Black | 0.5 | 0.5 | 0.5 | 0.5 |
Total | 100 | 100 | 100 | 100 |
Screw speed (small prototype) | 38HZ | 38HZ | 38HZ | 38HZ |
Extrusion temperature Zone 1/Zone 2 | 100/110 | 100/110 | 100/110 | 100/110 |
Gloss | 9.4% | 4% | 3% | 2.8% |
Surface | smooth | exquisite | exquisite | exquisite |
illustrate:
- Fast feeding speed, low extrusion temperature, good and stable matting effect.
- Polyesters from different manufacturers have different gloss, leveling, and gel time (Storage). It is recommended to test several polyesters.
3.The addition of accelerators may cause gloss increase and leveling deterioration. It is recommended to test it in a small test.
- Please pay attention to storage stability in hot summer. VI. Packaging and storage Kraft paper bag (polyethylene lining), 25Kg/bag. Store in a cool and dry place, away from fire and heat source